Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
You could do it with an inner mould as well as a compression mould. Clamp the moulds together with some wood as a load spreader and wind up the load. That way when it's cured you will get a gloss finish on both sides of the angle.