	Group: Forum Members 	        
    Posts: 460, 
    Visits: 5.2K 
    
 
          
		     | 
				                       
                 
                
                    
			            Hi Struan Welcome to the forum! Where about are you in Scotland?  You can certainly use 3D printing for the tooling, especially for room temp wet lay and infusion. There are materials that can go to higher temps if you want to do prepreg work but you can get pretty good results from infusion, and if need be clear coat the parts afterwards.
                  
			            				
			                                 
                     
                                            
                         
                    
                  
             |