			            Typically you would want something like a 200gsm (or similar, eg 210gsm we sell) cloth for the surface layer and some backing reinforcement.  If it is supporting the weight of the LED lights, perhaps around a mm thick which would be 4 layers of a typical 200g cloth or less layers if you back up with a thicker cloth.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |