Most paints once fully cured are ok. It is possible you may get some movement with oil based paints as they take a long time to fully cure.  You could seal the surface to be safe or conduct a small test piece with the paint you are using.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Harry94
H
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 5, Visits: 21
Hello I am going to use the GlassCast 50 on a 3D picture frame I am going to pour the max amount in one pour (25mm) my question is what paint can I use before I pour the GlassCast 50 on to. I don’t want any funny chemical reaction with the paint as you will be able to see it through the GlassCast. Should I put a varnish onto the paint before I pour the GlassCast 50 and if so is there anything particular I should use? Many thanks.