By Harry94 - 1/27/2020 10:44:36 PM
Hello I am going to use the GlassCast 50 on a 3D picture frame I am going to pour the max amount in one pour (25mm) my question is what paint can I use before I pour the GlassCast 50 on to. I don’t want any funny chemical reaction with the paint as you will be able to see it through the GlassCast. Should I put a varnish onto the paint before I pour the GlassCast 50 and if so is there anything particular I should use? Many thanks.
|
By Warren (Staff) - 1/28/2020 4:34:58 PM
Most paints once fully cured are ok. It is possible you may get some movement with oil based paints as they take a long time to fully cure. You could seal the surface to be safe or conduct a small test piece with the paint you are using.
|
|