+x f1rob - 1/26/2020 5:17:31 PMI would say bag looks marginal on size Both diameter and lengh.That's not to say you couldn't do it with the bag you have but just makes it more difficult !If its a good bag and you haven't done anything silly the leaks in your tape, give yourself a bit longer bag to bring your tape out further so it's easier to work on.Any bolts etc double breatherThe bag will go in the sharp corners but you need plenty of spare,pull a partial vac then work your bag around the job dont try to push in to the corners when its fully vacuumed. Get a water sprayer an spray your bagMakes it a LOT more supple