Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Yeh sure, I know basalt well, I only ask because most people are using it for cosmetic purposes. I have had similar experience to you though, I find it's interlaminar bond strength very poor - I was getting full fibres peeling off in strips rather than little bits like you have experienced. I always just put it down to the specific material that I was using, so it's interesting you have come to the same conclusion with a different supplier.
|