Group: Forum Members
Posts: 107,
Visits: 504
|
i bought a leak detector and to be honest it was'nt that dear, it is very good, came with a short pipe that attaches to the end for doing localised checks and a parabolic dish. it does find the smallest leaks.
i first used some ear defenders with a small hole drilled in 1 ear cup then pushed a tube inside, it worked ok but the leak detector can hear well out of our hearing range
|