Which glue do I use to bond two pieces of PTFE?


Author
Message
YouStoleMyMash
Y
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 8, Visits: 195
I need to bond two parts of PTFE together and, due to the non-stick nature of the material, I was wondering which glue/adhesive to use.

Thanks in advance
Reply
YouStoleMyMash
Y
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 8, Visits: 195
Hanaldo - 12/9/2019 10:45:18 AM
Depends on the end application, what are you trying to achieve? 

Speak to Permabond. They make a range of adhesives for bonding PTFE, they will be able to recommend the most suitable product.

Basically, I have a 8mm sheet that I've been using to make myself some dibbers. But now I want to make one that is thicker but don't want to fork out for a thicker sheet. 