Which glue do I use to bond two pieces of PTFE?


Author
Message
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
f1rob - 12/10/2019 3:53:14 PM
scottracing - 12/9/2019 10:52:33 PM
why dont you drill a couple of holes in the sheets and pin them together with nylon/PTFE dowels?


Tried to message you a couple of times mate but apparently you message box is full !

hi mate, ive deleted a load out now, i didnt realise there was a limit! Too much gassing eh Smile

f1rob
f1rob
Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
scottracing - 12/9/2019 10:52:33 PM
why dont you drill a couple of holes in the sheets and pin them together with nylon/PTFE dowels?


Tried to message you a couple of times mate but apparently you message box is full !

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
why dont you drill a couple of holes in the sheets and pin them together with nylon/PTFE dowels?


YouStoleMyMash
Y
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 8, Visits: 195
Hanaldo - 12/9/2019 10:45:18 AM
Depends on the end application, what are you trying to achieve? 

Speak to Permabond. They make a range of adhesives for bonding PTFE, they will be able to recommend the most suitable product.

Basically, I have a 8mm sheet that I've been using to make myself some dibbers. But now I want to make one that is thicker but don't want to fork out for a thicker sheet. 

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Depends on the end application, what are you trying to achieve? 

Speak to Permabond. They make a range of adhesives for bonding PTFE, they will be able to recommend the most suitable product.
YouStoleMyMash
Y
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 8, Visits: 195
I need to bond two parts of PTFE together and, due to the non-stick nature of the material, I was wondering which glue/adhesive to use.

Thanks in advance