why does the bag loosen up when resin starts flowing???


Author
Message
Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
I'd bet that the cleaning removed the spray adhesive from the surface and left you with the spray texture on the part. What spray tack did you use and are you sure you didn't use too much of it? Some (most) of them don't completely dissolve in epoxy and leave traces on the surface. I like to use the isotacker from sicomin against the mould of visible parts, and then aerofix 2 for consecutive layers, as the tack is much better.
mscomposites
m
Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)Supreme Being (315 reputation)
Group: Forum Members
Posts: 23, Visits: 108
never tried that one, we are using the fibertack and applying a very thin coat just to hold the material in place. And then using es99 to hold the rest in place.