why does the bag loosen up when resin starts flowing???


Author
Message
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's caused by uneven vacuum inside the bag. Can you post a photo of your layup?
mscomposites
m
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 23, Visits: 108
Trying to figure out how to keep the bag to stay tight all the way through the infusion process. there’s absolutely no leaks before we start infusing the resin. But as soon as we open up the resin inlet line the inlet side/area of the bag loosens up and it really never get a tight until the resin starts to gel. Anyone have this issue or does anyone know how to fix this issue. I’m finding small pitting on the surface and only on the inlet side so i’m guessing g it’s happening from the bag being loose on that side.