Group: Administrators
Posts: 2.5K,
Visits: 8K
|
HI,
As long as you key the surface with sandpaper after it has gone fully hard then you should be fine. You could vary the MEKP ratio to make it take longer to cure but that would need to be experimented with to get it just right for the timings and temperature you are working at.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|