+x f1rob - 10/9/2019 7:26:11 PMWell you certainly live in the right area !Couple of companies do courses, dark matter composites but personally I dont rate themYou could do a lot worse than reading both of Keith noakes books ( bit dated now but still good)Simon mcbeaths composites:a practical handbookOr glassfibre handbook by r h warringGet some materialsJohn burn, silamid,alchemy,east coast composites,vac innovations an shdHave a playLots of stuff on YouTube but if you dont know the trouble is filtering the good from the badDepends how far you want to take it but you will learn more in a proper workshop ( an ways of doing things you hadnt even thought of) than you will with books and videos.