Turns out you can do it:
Faster thermoset prepreg cycles through improved heating are also being sought by Voetsch Industrietechnik GmbH in Germany. It developed an industrial microwave oven, called VHM Hephaistos, with a hexagonal chamber that is said to apply more homogeneous heating than a round chamber. This year saw its first commercial application for curing carbon-fiber/epoxy prepregs. The result was said to be faster cycles than with conventional autoclaves and greater energy efficiency because all the energy goes into the part while the chamber stays cool. More uniform heating is also said to cause less degradation of carbon fibers. Chamber sizes are up to 1.8 x 2 meters. Metal tools reportedly can be used.
|