posted 6 Years Ago
ANSWER
HOT
Topic Details
B
Group: Forum Members
Posts: 38,
Visits: 420
Bought this glasscast 3 for a project about 8 months ago and worked very well.
Mixed up a litre today by weight 100/50 as per instructions for 10 minutes. Steam started coming off and went totally solid a couple of minutes later....... really not happy !!!!!
Reply
Like
3
Reply
Bhamoggy
B
Bhamoggy
posted 6 Years Ago
ANSWER
HOT
Post Details
B
Group: Forum Members
Posts: 38,
Visits: 420
Eh???
I mixed enough for 80cm x 26cm and a 3mm depth.
I know glasscast 3 is only a thin surface resin and I’ve used it before successfully.
It was going onto a glasscast 50 pour which had 2 pours to reach a depth of 40mm.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Glasscast 3 no good
Bhamoggy
-
6 Years Ago
Who told you to mix it for 10 minutes? Epoxies don't need to be mixed for 10 minutes, 2-3 minutes should be plenty. Glasscast3 is a low volume coating resin. A litre of resin in the style of jug you...
Hanaldo
-
6 Years Ago
Mixed roughly for 10 minutes in total. Swapping jugs half way thru. This is how I’ve done it before with no issues and I’ve mixed glasscast 50 the same way without ever having problems
Bhamoggy
-
6 Years Ago
Yes, glasscast 50 is made for thicker pours and therefore less reactive and doesn't build up that much heat when mixed unnecessarily long in large batches. You can't do that wich glasscast 3. Unless....
oekmont
-
6 Years Ago
Eh???I mixed enough for 80cm x 26cm and a 3mm depth. I know glasscast 3 is only a thin surface resin and I’ve used it before successfully. It was going onto a glasscast 50 pour which had 2 pours to.....
Bhamoggy
-
6 Years Ago
80x26x0,3cm=0,62L. And 3mm is the Upper end. But that is not my point. You simply can not let epoxy stand around (or mix) in a compact 1L container. The reaction will build up heat, which accelerates...
oekmont
-
6 Years Ago
I see and I get what you’re saying however I followed the instructions correctly. There should be limitations written on the instructions as to what not to do then if this is the case. As far as I’m....
Bhamoggy
-
6 Years Ago
No, it is clearly advised to mix for 2x3min.
oekmont
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search