By Bhamoggy - 9/21/2019 10:17:06 AM
Bought this glasscast 3 for a project about 8 months ago and worked very well. Mixed up a litre today by weight 100/50 as per instructions for 10 minutes. Steam started coming off and went totally solid a couple of minutes later....... really not happy !!!!!
|
By oekmont - 9/22/2019 5:55:57 PM
No, it is clearly advised to mix for 2x3min.
|
|