Hey everybody,

I want to build a front wing depending on the original part with Prepreg. For sure it has to be a two part mould. My problem is how to get the two parts bonded because the edge line will be only about 1mm and so it is too small to make a bonding. I have some ideas and hope to get some input:

1. after making the two parts I go for a smaller version. I make a second carbon part using the first carbon Part as „mould“. This way I get a smaller part which can be used as connecting part to bond the two main parts together.

2. I lay up the two moulds with a little overlap on one part, put them together, insert a bladder and make a small hole on the downside to inflate the bladder. But actually I have never tried this technique. I get it in theory but I do not now what to use as bladder and how much pressure is necessary.

3. same as number two but using a silicone plug which should expand with heat and produce enough pressure for the Prepreg. In this case I would be happy to get some tips about how to make the silicone plug, especially where to get the right material.

4. last idea: filling each mould with polystyrene foam and use the foam to produce pressure. But I do not know if the foam will produce enough pressure and how to fix the flaps.

So you See, lots of questions :] perhaps some of you understand what I try to do and give me some input.

Have a nice Weekend!
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That looks more of a splitter than conventional aerofoil.  If the detail is important on both sides, then in effect take a mould of each side and lay it up in 2 halves and bond together.  If you are careful in the moulding, you may be able to create a bonding lip or joggle on one half to give a nice bonding surface area.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
SHaas
S
Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)
Group: Forum Members
Posts: 46, Visits: 383
Do you have an idea how to make such a lip in the mould? You Said make it careful which is a good advice, but I am not sure how to do that...
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
SHaas - 6 Years Ago
Hanaldo - 6 Years Ago
SHaas - 6 Years Ago
Hanaldo - 6 Years Ago
SHaas - 6 Years Ago
Warren (Staff) - 6 Years Ago
SHaas - 6 Years Ago
Hanaldo - 6 Years Ago
SHaas - 6 Years Ago
     No more ideas?
SHaas - 6 Years Ago
MarkMK - 6 Years Ago
SHaas - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search