Hey everybody,

I want to build a front wing depending on the original part with Prepreg. For sure it has to be a two part mould. My problem is how to get the two parts bonded because the edge line will be only about 1mm and so it is too small to make a bonding. I have some ideas and hope to get some input:

1. after making the two parts I go for a smaller version. I make a second carbon part using the first carbon Part as „mould“. This way I get a smaller part which can be used as connecting part to bond the two main parts together.

2. I lay up the two moulds with a little overlap on one part, put them together, insert a bladder and make a small hole on the downside to inflate the bladder. But actually I have never tried this technique. I get it in theory but I do not now what to use as bladder and how much pressure is necessary.

3. same as number two but using a silicone plug which should expand with heat and produce enough pressure for the Prepreg. In this case I would be happy to get some tips about how to make the silicone plug, especially where to get the right material.

4. last idea: filling each mould with polystyrene foam and use the foam to produce pressure. But I do not know if the foam will produce enough pressure and how to fix the flaps.

So you See, lots of questions :] perhaps some of you understand what I try to do and give me some input.

Have a nice Weekend!
Reply
SHaas
S
Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)
Group: Forum Members
Posts: 46, Visits: 383
Do you have an idea how to make such a lip in the mould? You Said make it careful which is a good advice, but I am not sure how to do that...
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
SHaas - 6 Years Ago
Hanaldo - 6 Years Ago
SHaas - 6 Years Ago
Hanaldo - 6 Years Ago
SHaas - 6 Years Ago
Warren (Staff) - 6 Years Ago
SHaas - 6 Years Ago
Hanaldo - 6 Years Ago
SHaas - 6 Years Ago
     No more ideas?
SHaas - 6 Years Ago
MarkMK - 6 Years Ago
SHaas - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search