Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Where you need to overcoat, you will need to key with 120 grit paper and give it a clean before pouring again. There will be a very slight seam line on the edge of the new pour, but this can be sanded out and polished back to a gloss finish once the pour has gone hard.