Be very careful when sanding that you don't go into the fabric itself as if you do, it can ruin the cosmetic effect. Remove only a small amount of material at a time then reassess to see how it looks. I would try polishing first and see how it looks before getting aggressive with the sanding.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|