HI ALL,
im asking for the second opinion. right now my final bagging sequence are 1-layer of peel ply 5-layer of glass cloth (at specific area) 1-layer of NP 1 layer of glass cloth (all area) 2 layer of N10 1-layer of bagging film. the idea of 5 layers of glass cloth is to absorb extra resin on that specific area to make it thinner. the problem I faced is only 2 layer of glass cloth are absorbing the resin, the 3 layers didn't absorb any resin what can I do to make the resin bleed more so that all the glass cloth absorb the resin?
|