Hi all, see video, this is the main pivot part of the rear suspension on a bike, the alloy part has come loose and I need to sort it obviously it needs to be extremely strong to cope with jumps ect, what should I be using and how strong would the bond be ?

Any advice appreciated.


Replies
Brokenframeguy
B
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 5, Visits: 7
Thank you Rich Ill get that, what do you recommend to degrease with ? I have some brake/clutch cleaner and have a few bottles of isopropyl alcohol, would these be sufficient ?
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Brokenframeguy - 7/16/2019 4:20:34 PM
Thank you Rich Ill get that, what do you recommend to degrease with ? I have some brake/clutch cleaner and have a few bottles of isopropyl alcohol, would these be sufficient ?

IPA is perfect