Brokenframeguy
B
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 5, Visits: 7
Hi all, see video, this is the main pivot part of the rear suspension on a bike, the alloy part has come loose and I need to sort it obviously it needs to be extremely strong to cope with jumps ect, what should I be using and how strong would the bond be ?

Any advice appreciated.


Reply
Brokenframeguy
B
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 5, Visits: 7
A update as promised, after 3 pretty rocky rides theres no problems so far so thanks again Rich. 

 

PS:The bikes a Yeti 575 if anyone finds this from googling how to fix one. 