Hello there guys !
I am doing some skinning works with CF and until now I've been using a 2 part black by color brushable adhesive and everything was amazing but now they discontinued the product, so I found myself in a situation. Can someone help me with some alternatives to obtain a perfect bond before using the resin with the parts ? 
Some of the parts have shapes(see attached picture) and I really don't want to find myself in a awkward situation finding them with the fabric apart the part at corners the next day. I did a little research but I have found nothing similar to this product I've been using.
Any suggestion is appreciated.
Thank you !
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No, not by the sounds of it. But it will achieve the same objective of tacking the fabric into place, you will just have to get used to different application techniques. 

Watch the Easy Composites XCR skinning video on YouTube, you will see how it works.