Hello there everyone. I bought a resin having the mixing ratio 100:2. I was wondering if using half I will use 50:1 or less 25:0,5 ? It is correct ?
Thank you !
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
mdoru - 5/17/2019 10:21:04 AM
Hello there everyone. I bought a resin having the mixing ratio 100:2. I was wondering if using half I will use 50:1 or less 25:0,5 ? It is correct ? Thank you !

Sounds right.

Is it a polyester or vinyl ester catalyst?





mdoru
m
Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 162
It is polyester.
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Ratio is a ratio, it doesn't change. 100 parts Part A to 2 parts Part B is the multiplier and can be applied to any number you like. It simply means for every 100 parts of resin you have, you need 2 parts of hardener. Eg. If you bought a 5kg kit and you were mixing up 4kg you would need 4000÷1.02, hence you would measure out 3921g of resin and 79g of hardener. If you needed to mix up 2kg you would need 2000÷1.02, hence 1961g of resin and 39g of hardener. You can use this for any amount of resin, but your ratio is always 100:2.
mdoru
m
Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 162
Thanks a lot ! So if I mix 50grams of resin I’ll use 49 A and 1 B
Edited 7 Years Ago by mdoru
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
mdoru - 5/17/2019 11:46:28 AM
Thanks a lot ! So if I mix 50grams of resin I’ll use 49 A and 1 B

Unless I'm doing it wrong all the time it should be 50+1 
But with polyester Resin and catalyst it shouldn't be to much of a problem not being 100% accurate 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




JasonFL
JasonFL
Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)
Group: Forum Members
Posts: 51, Visits: 707
A rule of thumb I use with Poly or Vinyl is 5 cc MEKP per half liter. 10cc if using tooling gelcoat.

You really don’t need to be super accurate with poly or vinyl because they only need catalyst to speed up the cure rate. Poly will cure on its own without MEKP (in like 100 years).

If you mess up and your part is not curing move it to a hot room, and last ditch effort put it out in the sun.

Jason
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I have always mixed catalyzed resins as 100g + 1ml for 1%, technically incorrect but bloody close, these resins adjustable % anyway and not a fixed ratio like other resins.

Also makes the calculation really easy and less risk of mix mistakes.

For 1% ratio 1kg of resin is 10ml of catalyst.

100g is1ml
5kg is 50ml

Using mls with squeeze type catalyst dispensers.




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search