By mdoru - 5/17/2019 10:21:04 AM
Hello there everyone. I bought a resin having the mixing ratio 100:2. I was wondering if using half I will use 50:1 or less 25:0,5 ? It is correct ? Thank you !
|
By Fasta - 5/20/2019 2:36:08 AM
I have always mixed catalyzed resins as 100g + 1ml for 1%, technically incorrect but bloody close, these resins adjustable % anyway and not a fixed ratio like other resins.
Also makes the calculation really easy and less risk of mix mistakes.
For 1% ratio 1kg of resin is 10ml of catalyst.
100g is1ml 5kg is 50ml
Using mls with squeeze type catalyst dispensers.
|
|