When drilling into Carbon or FRP panels. I’m aware that stepping your drill bits up to the size you want will give you clean edges rather than frayed. So beyond that basic step my question is below...

I know there’s charts online, but In your experience, what RPM do you set your drill press to for drilling glass/carbon/Kevlar?

Jason
Reply
JasonFL
JasonFL
Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)Supreme Being (341 reputation)
Group: Forum Members
Posts: 51, Visits: 707
Thanks! Thats what I’m attempting to drill, but it was room cure Carbon Kevlar.

Jason
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search