Hi, I recently bought a 5k tub of epoxy moulding paste and hardener as part of an order. When I opened the tub to use it today the paste was rock hard. I had already coated my parts with the epoxy tooling gel coat so I cut some of the paste out with a knife to attempt to use it. I thought the hardener may soften the paste to enable me to use it. After about 15 minutes of mixing I had to use the paste as the gel coat was setting. Even though I had worked the paste it still had hard lumps in it which I’m sure will affect the outcome of the mould. So, the question is, is there something I can use to revive the paste or do I need to send it back to you? Just to confirm, I bough the paste & gel coat with their hardeners last week and broke the seal on the paste tub today. I have previously used your moulding paste and it was very pliable, like paste I suppose. I’m just hoping all my hard work setting up the work piece hasn’t been in vain! Please advise me of my options, Regards Roger
|