Seams in carbon fiber surface


Author
Message
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Ok I know it has been done but I don't know how yet. When you look at some really nice carbon pieces often you see a nice joint between two pieces of carbon that has been placed in the mold. It is obviously not just cut with a pair of scissors and layed down.

Are the two pieces stitched together like  seam in clothing. So that once layed down the frayed edges don't show because they are inside the laminate?

Lets say you are going to place your carbon cloth in a bowl shaped mold. If you cut your carbon in triangular shapes and put them in your mold you would have a freyed look at the joints.

Any advice.

Thanks

Fred 
Replies
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
this is done by using either pre-preg or a product called pro finish carbon cloth... https://www.easycomposites.co.uk/200g-profinish-coated-22-twill-3k-carbon-fibre-cloth 
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Well thank you very much. The prepreg did occurr to me but the other stuff you mentioned I didn't know existed.

Thats great news and I will have to try it. I suppose carbon tape over the seams would work as well.

Fred 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search