Hi guys been skinning for a while now and I'm looking for the best resin that has the highest temp rating without post curing the parts.. I see the el2 laminating resin is higher than the xcr resin and even more if the slow hardner is used..
I didn't get on with the xcr resin before,  pinholes and clear coating it was a nightmare!!
Also needs to be bubble free and crystal clear..
My process is tack spray carbon to the piece.. wet it out and then I'm vac bagging the part.
Thanks
Reply
CmCarbon
C
Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)Supreme Being (168 reputation)
Group: Forum Members
Posts: 19, Visits: 239
I don't have the means to post cure unfortunately.
What's the next best resin you stock? 
Also does your fusion spray only dissolve in epoxies resins not poly resins? 