|
Group: Forum Members
Posts: 19,
Visits: 239
|
Hi guys been skinning for a while now and I'm looking for the best resin that has the highest temp rating without post curing the parts.. I see the el2 laminating resin is higher than the xcr resin and even more if the slow hardner is used.. I didn't get on with the xcr resin before, pinholes and clear coating it was a nightmare!! Also needs to be bubble free and crystal clear.. My process is tack spray carbon to the piece.. wet it out and then I'm vac bagging the part. Thanks
|