Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi so a while ago I've worked on a project using
grey poly/carbon twill
and Soric Lantor infusion medium.
I wasn't that happy about the result coming out of the mould and want to know why, So I won't make the same mistake next time.
1. So my first guess is some air went through the part? but the bag was fully sealed and tested with a drop test of 45min and so on.
No air could have passed through the mould because the mould was totally inside the vacuumbag.
2. mould surface was not perfect giving it orange peel look? The mould was pollished and very shinny so not possible too, I guess.
3. I've used a polyester gelcoat and epoxy infusion resin (reason, Polyester mould, Polyester gelcoat (won't stick to the mould, epoxy would stick way more) and epoxy infusion resin bonds
well to polyester so thats why, but maybe there is a reaction between the 2?!
You can watch the small video on how it was made, maybe you can find some errors in the video?!
Please share you'r ideas i'll be happy to hear every possible theory
Kind regards,
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
Replies
r0bsk1
r0bsk1
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 38,
Visits: 307
I always thought you couldnt vacuum polyester as it boils. There's a chemical reaction releasing gas too.
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
No went well in the past with polyester.
Already did different parts with a polyester infusion resin.
Never had problems with it, main reason I'm more for the epoxy now is that it
is more transparant, stronger (in theory, never tested it) and I don't have the smell anymore.
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Question on finished product with soric
matthieutje65
-
13 Years Ago
Well judging by the video, you applied poly gelcoat, placed the fabric on the tacky gel and then...
baja_patient
-
13 Years Ago
I always thought you couldnt vacuum polyester as it boils. There's a chemical reaction releasing gas...
r0bsk1
-
13 Years Ago
No went well in the past with polyester. Already did different parts with a polyester infusion...
matthieutje65
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search