+x scottracing - 3/15/2019 10:56:13 PMStretchlon is pretty good for this application. Although i don't like the stuff personally use normal bag but wet it out with a water spray bottle to make it more malleablehttps://www.tygavac.co.uk/stretchlon-200
+x CmCarbon - 3/16/2019 1:41:07 AM+x scottracing - 3/15/2019 10:56:13 PMStretchlon is pretty good for this application. Although i don't like the stuff personally use normal bag but wet it out with a water spray bottle to make it more malleablehttps://www.tygavac.co.uk/stretchlon-200That looks really good.. wonder if they sale samples to try