By CmCarbon - 3/15/2019 11:20:21 AM
Hi guys looking to order a few things.. what's the best vac bagging material to use that will stretch alot as parts I'm skinning has alot of detail.. I used the red one before and it was ok.. it wont be in a oven if that makes a difference. Cheerz
|
By CmCarbon - 3/16/2019 11:30:25 AM
I use peelply and a breather cloth over my parts so should be ok buddy
|
|