Hi, do you have any images of a cured part using the red poly/carbon twill please?

The red in my current fabric goes very dark once wetted and cured. I need something that maintains a bright red. I've found a fabric in the US but would be best not to import it.

Cheers
Reply
r0bsk1
r0bsk1
Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)
Group: Forum Members
Posts: 38, Visits: 307
Blue and green didnt change that much at all but red almost disappeared.

So to create a light back ground would it mean creating the initial CF part with a white pigment in the resin and then to wrap the the part in the red CF?

Or lose the white pigment but use a white backing coat for the red CF to be wrapped?

Either way i dont see a way to avoid wrapping