By r0bsk1 - 11/2/2012 12:50:26 PM
Hi, do you have any images of a cured part using the red poly/carbon twill please?
The red in my current fabric goes very dark once wetted and cured. I need something that maintains a bright red. I've found a fabric in the US but would be best not to import it.
Cheers
|
By matthieutje65 - 11/8/2012 11:17:07 AM
Thanks for the information, looks true by seeing images on the internet of "Red Kevlar"
|
|