Oakemont, we actually got a quite a variety of resin uptake figures for soric in our own testing and calculating from customers figures - with the manufacturers quoted figure being fairly conservative in our experience. Especially as a lot of people making cosmetic parts will leave the resin feed open for longer than usual to help avoid pinholes. Of course making it resin rich in this way effects the fibre/resin ratio as well as the resin uptake. An accurate and fair comparison would only work exactly on a like for like basis. I imagine Lantor's test figures will be for a standard infusion done a set way hence being towards the lower end of the resin uptake we have seen.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|