Soric/Resin Ratios?

http://www.talkcomposites.com/Topic32119.aspx

By HansenJC - 2/21/2019 2:53:42 AM

We all know the desired ratios of CF to resin and we know the achievable ratios differ between hand layup/vacuum bagging, and Resin Infusion... but what is the ideal and actually achievable ratio for Soric/Resin when done as part of a Resin Infusion that has CF skins? Are there any good published data for Soric/Resin design ratios?
By oekmont - 2/22/2019 1:02:36 PM

My experiments only differed by 5% and were within 10% of the data from my supplier. Lrc1.5 took a little less resin, lrc3 a little more and sf3 a little less in my setup. 5 repetitions per material.