Would there be any disadavantsges in using glasscast 10 to seal the edge of wood prior to using glasscast 50. This is to reduce the time between sealing and the main pour as the 10 is a faster cure resin. But I I don’t want this if adhesion or wood penitration is inferior.
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
No problem at all doing that.  GlassCast 10 and 50 use the same resin just with different speed hardeners.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search