In my search for polyurethane boards to make a plug, I am looking for low density. Approximately 4 to 6 Lbs. Cubic Ft (64 to 96 KG/Cu Meter) I have found a few off-shore suppliers including one each in UK, and Canada. I have made inquiries on pricing vie email or web response forms but I am not getting responses from the USA supplier after I was referred to them by the manufacturer. I would prefer finding a USA supplier to avoid the high cost of shipping and any possible duties or import restrictions. Can anyone please point me to a responsive supplier in the USA for this material?
For reference and perhaps to answer one key question, I do all of my research via the internet at night because I work during the day, so phone conversations is not an option for me.


A Lifelong Learner

Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Contact building supply companies. Closed cell rigid polyurethane foam is often used in the building industry for insulation.
John Hansen
J
Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)
Group: Forum Members
Posts: 42, Visits: 232
Hanaldo - 2/12/2019 7:02:13 AM
Contact building supply companies. Closed cell rigid polyurethane foam is often used in the building industry for insulation.

It seems that in the USA the commonly available rigid board insulation is polystyrene. And i thought I have read that Polystyrene would not be compatible with the various resin materials used for making molds.
Any experience in making plugs here in the USA would be appreciated.


A Lifelong Learner

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
HansenJC - 6 Years Ago
Hanaldo - 6 Years Ago
HansenJC - 6 Years Ago
Hanaldo - 6 Years Ago
HansenJC - 6 Years Ago
tpenfield - 6 Years Ago
k.alan.bates - 6 Years Ago
JasonFL - 6 Years Ago
Noah Lieske - 6 Years Ago
explorecomposites - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search