Sourcing Polyurethane boards in USA for making plug


Author
Message
John Hansen
J
Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)Supreme Being (403 reputation)
Group: Forum Members
Posts: 42, Visits: 232
In my search for polyurethane boards to make a plug, I am looking for low density. Approximately 4 to 6 Lbs. Cubic Ft (64 to 96 KG/Cu Meter) I have found a few off-shore suppliers including one each in UK, and Canada. I have made inquiries on pricing vie email or web response forms but I am not getting responses from the USA supplier after I was referred to them by the manufacturer. I would prefer finding a USA supplier to avoid the high cost of shipping and any possible duties or import restrictions. Can anyone please point me to a responsive supplier in the USA for this material?
For reference and perhaps to answer one key question, I do all of my research via the internet at night because I work during the day, so phone conversations is not an option for me.


A Lifelong Learner

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
HansenJC - 7 Years Ago
Hanaldo - 7 Years Ago
HansenJC - 7 Years Ago
Hanaldo - 7 Years Ago
HansenJC - 7 Years Ago
tpenfield - 7 Years Ago
k.alan.bates - 7 Years Ago
JasonFL - 7 Years Ago
Noah Lieske - 7 Years Ago
explorecomposites - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search