Thanks Rich,
I jetted off to Europe before the owner got to see it in person (only finished it the day before leaving), but he has seen photos and the feedback I got was that he loves it haha.
And yeh, everyone is happy with the 20kg weight saving. Unfortunately the fibreglass bootlid still weighs 7kg, so hopefully we can talk the owner into getting on to that as soon as I'm back. It feels like a huge waste when you can lift the whole rear clam including lights and rear wing with one hand, and then you put the boot lid back on and it's almost back to a two person job!
|