Yeh can be tricky to keep the back smooth. I would try placing a separate small piece of release film over the paper and make sure that it goes on smooth with no wrinkles. May also help to use some flash breaker tape all around that piece of release film to prevent any resin bleed underneath, though that likely won't be a problem anyway. Then proceed as you usually do with the layup.
|