By Derek Dunning - 2/11/2019 12:58:54 PM
Afternoon, thanks for the Youtube videos, helped me alot getting started with infusion.
The question I have is how do people add full colour images to fibreglass parts and on top of carbon parts?
Thanks for any help with this.
Cheers D.
|
By Hanaldo - 11/4/2020 4:50:05 AM
Yeh can be tricky to keep the back smooth. I would try placing a separate small piece of release film over the paper and make sure that it goes on smooth with no wrinkles. May also help to use some flash breaker tape all around that piece of release film to prevent any resin bleed underneath, though that likely won't be a problem anyway. Then proceed as you usually do with the layup.
|
|