As stated I am completely new at this.
For the past 10 years I have been having these made out of 26 gauge steel panels.

My thought is that I could use these steel panels as a mold and press the shape out of fiberglass.



I am completely new at this so I will start with some basic questions.

  Is it possible?

  The final panels at 40x48 and made out of a full 4x8 foot sheet. How much fiberglass would you need to make a similar panel.

Thank you in advance and I know I will have more questions.

Reply
artistwantab
a
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 25
Still looking for some insight on materials.

Resins... Can you recommend a resin?
       I currently use TotalBoat High Performance Epoxy Resin for woodworking.  Will this also work for fiberglass?
chemical release agent? Recommendation?
Fiberglass recommendation?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
artistwantab - 6 Years Ago
Warren (Staff) - 6 Years Ago
artistwantab - 6 Years Ago
artistwantab - 6 Years Ago
Warren (Staff) - 6 Years Ago
artistwantab - 6 Years Ago
Steve Broad - 6 Years Ago
artistwantab - 6 Years Ago
Steve Broad - 6 Years Ago
Zorbit - 6 Years Ago
artistwantab - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search