Group: Forum Members
Posts: 6,
Visits: 45
|
I can see a couple of problems here. First, you will have to "roll" the top metal sheet onto the bottom sheet whilst feeding the glass mat in from the open end, otherwise the glass will not be able to slide fully down into the bottom of the valleys and will tear. Second, it's going to be really difficult to get even clamping over the whole area unless you use a vacuum system, the pressure required to get that length of glass into so much corner will add up to quite a lot, enough to bow the metal, although perhaps you could cover it with sandbags to get distributed pressure.
|