The EasyGloss is a brilliant product, it really is. Applied properly (with a good machine polisher and a soft black pad), it will add an extra gloss and depth to finished parts.
As for the UV protection, that's really anyone's guess - it's too new a product for anyone to have any actual data on that. Realistically, it is a wax and will work the same as automotive protective waxes. It will add a little bit of protection, and will need fairly regular treatment to last as long as possible, it's not a case of apply it once and have a UV resistant part for 20 years. It's also going to depend a lot on the specific resin that your pre-preg is using, some are much more sensitive than others. The X-Preg is very good for an epoxy, all the parts I have made with it are still as good as the day I pulled them out of the mould. The old EasyPreg wasnt quite as good, a lot of those parts I made have lost their gloss a bit and require more regular treatment with the EasyGloss.
Personally, I like the EasyGloss and it's a bit of added protection. There is no real guarantee that clear coats provide any more protection than that either, it is very subjective. It's best to be realistic and accept that all resins are UV sensitive plastics, and will not last forever.
|