Group: Forum Members
Posts: 338,
Visits: 2K
|
If absolute detail wasn't too much of an issue, you could try covering the hole thing in 1mm sheet wax. It's quite conformable, especially with a bit of help from a heat gun. Of course. the surface wouldn't be glossy and the finished part would be 1mm bigger but it would allow things to release properly, if other coatings on your 3D part aren't suitable.
Failing that, you could try to re-create your part in silicone, first creating a silicone mould and then a copy of the part. This would then release okay.
|