Vacuum bagging gone wrong?


Author
Message
Dimitar
Dimitar
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 3, Visits: 18
Hi there,

My friend and I received help with regards to vacuum bagging from Paul at Easy Composites yesterday and I can't recommend him enough, valuable advice and very helpful!

It came time to de-bagging today and our finished product hasn't turned out as we expected. I've attached some pictures, what could we have done wrong?

We used some temporary adhesive so that may be the murkiness of the top-most layer, but along the edges of the part there seems to be just lines of glue. Could this indicate that the cloth wasn't properly pressed into all the crevices at the time of bagging, too much resin, wrong curing temperature? 

Last night when we got back home it looked like the bag was still under vacuum. We placed an electric blanket underneath and then covered the part with the breather cloth. I think it may have been better to use a duvet as it didn't seem too warm when I went in the garage this morning.

Any help would be appreciated!
P.S. we bagged at 5pm yesterday and de-bagged today at 19:00 having used the Fast hardener.




Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Ok. The Soric wont be helping your bridging issues here - you are trying to make it conform to too tight a corner. Make a template and cut the Soric so that it fits inside the component you are making and doesnt have to overlap onto the flange.